Specification
Incl. MTC acc. EN 10204 / 3.1 with all mechanical and chemical properties. MTC has to be send before delivery by E-Mail from each product to control through QD of FER Kladno
Specification valid for W.Nr. 1.1191 – C45E / 1.1201 – C45R ( „S“ 0,020-0,030 % )
MATERIAL DESCRIPTION: | W.Nr. 1.1191 / 1.1201 acc. EN 10083 : 2007 |
Heat Treatment: | normalized acc. EN 10083, EN 10250, SEW 550 (or requirement +A, +QT) |
Grain size: | 5 and finer acc. ASTM E 112 |
Microcleanliness: | K4 max.30 acc. DIN 50602 |
US Testing: | 100% acc. EN 10228-3 / cl.3 |
Forging ratio: | forged min.3,5 / rolled min.5 |
Weight piece/bundle: | max. 20000 kg |
Chemical composition acc. EN 10083: 2007
C | Si (max) | Mn (max) | P (max) | S (max) | Cr | Ni | Mo | Cr+Mo+Ni |
---|---|---|---|---|---|---|---|---|
0.42 - 0.50% | 0.15 – 0.40 | 0.60 – 0.80 | 0.030 | 0.030 | 0.030 | 0.40 | 0.10 | 0.63 |